Dab tsi yog qhov kub siab tshaj plaws ntawm silicone pwm?

Silicone pwm tau dhau los ua cov cuab yeej tseem ceeb hauv ntau qhov kev lag luam vim lawv qhov ntsuas kub zoo heev. Nws daim ntawv thov dav dav hauv kev ua zaub mov, kev tsim khoom siv kho mob, kev tsim khoom siv hluav taws xob, thiab lwm yam kev lag luam yog vim kev ua haujlwm ruaj khov ntawm silicone pwm hauv qhov kub thiab txias. Nrog rau kev nce qib ntawm kev siv thev naus laus zis, peb ntseeg tias silicone pwm yuav ua lub luag haujlwm tseem ceeb rau yav tom ntej, ua tau raws li qhov xav tau ntawm ntau yam kev lag luam rau kev ua haujlwm siab thiab kub resistant pwm.
1. Kev qhia yooj yim ntawm silicone pwm
Silicone pwm yog cov pwm ua los ntawm silicone roj hmab ua lub substrate, uas muaj qhov yooj yooj yim, tshuaj stability, thiab txhua yam muaj zog. Vim nws cov kev ua tau zoo heev, silicone pwm yog dav siv nyob rau hauv ntau lub teb, xws li khoom noj khoom haus, kev kho mob khoom tsim, hluav taws xob cov khoom, thiab lwm yam.
2. Cov yam ntxwv kub tsis kam ntawm silicone pwm
Cov yam ntxwv ntawm qhov kub thiab txias ntawm silicone pwm feem ntau yog nyob ntawm qhov kev ua haujlwm kub ua haujlwm ntawm silicone roj hmab. Silicone roj hmab yog qhov kub-kub elastomer, thiab nws qhov kub-kub kuj tso cai rau cov pwm silicone kom ruaj khov lub cev thiab tshuaj lom neeg nyob rau hauv qhov kub thiab txias. Feem ntau hais lus, qhov kub tsis kam ntawm silicone pwm feem ntau yog nyob nruab nrab ntawm -50 degree C thiab 250 degree C, uas ua tau raws li ntau yam kev lag luam xav tau.
Kub kub stability ntawm silicone roj hmab
Silicone roj hmab muaj kev ruaj ntseg zoo heev, thiab txawm tias nyob rau hauv qhov kub thiab txias, silicone pwm tuaj yeem tswj lawv cov duab thiab elasticity. Qhov no ua rau daim ntawv thov ntawm silicone pwm ntau heev nyob rau hauv high-temperature ib puag ncig. Piv txwv li, thaum ci zaub mov, silicone pwm tuaj yeem tswj lawv cov duab ruaj khov yam tsis muaj deformation lossis melting.
2. Kev tiv thaiv kub kub hloov pauv
Silicone pwm kuj muaj qhov kub thiab txias. Txawm tias nyob rau hauv ib puag ncig nrog kev hloov kub ceev, silicone pwm tuaj yeem tswj tau lawv qhov kev ruaj ntseg thiab tsis tshua muaj kev tawg lossis deformation. Cov cuab yeej no ua rau cov pwm silicone ua tau zoo hauv kev tsim cov txheej txheem uas yuav tsum tau hloov qhov kub thiab txias, muab kev yooj yim rau kev tsim khoom.
3. Daim ntawv thov ntawm silicone pwm nyob rau hauv txawv teb
Qhov ntsuas kub tsis kam ntawm silicone pwm txiav txim siab lawv daim ntawv thov dav hauv ntau qhov chaw. Cov hauv qab no yog qee qhov chaw siv tau zoo:
1. Kev ua zaub mov
Hauv kev lag luam ua zaub mov, silicone pwm tau dav siv rau kev ci, ua cov qhob noom xim kasfes thiab cov khoom qab zib, thiab lwm yam. Nws qhov kub tsis kam ua kom zoo thiab kev nyab xeeb ntawm cov zaub mov.
2 Kev tsim khoom siv kho mob
Silicone pwm feem ntau yog siv rau hauv kev tsim cov khoom siv kho mob, thiab lawv qhov kub thiab txias ua kom muaj kev ruaj ntseg ntawm cov cuab yeej thaum kub kub kom tsis muaj menyuam.
3 Kev tsim khoom siv hluav taws xob
Hauv kev tsim cov khoom siv hluav taws xob, cov pwm silicone feem ntau yog siv los ua cov sealing thiab insulating Cheebtsam nyob rau hauv high-temperature ib puag ncig, kom ntseeg tau tias cov khoom siv hluav taws xob nyob rau hauv ntau yam kev ua haujlwm.
Dab tsi yog qhov kub siab tshaj plaws ntawm silicone pwm?
Feem ntau, qhov kub siab tshaj plaws ntawm silicone pwm yog nyob ib ncig ntawm 250 ° C. Qhov txiaj ntsig no yuav txawv ntawm cov qauv tshwj xeeb thiab kev tsim cov txheej txheem ntawm silicone roj hmab, tab sis nyob rau hauv feem ntau ntawm daim ntawv thov scenarios, qhov kub tsis kam ntawm 250 ° C yog txaus. kom ua tau raws li qhov yuav tsum tau ua.