1. txheej txheem ntws
Extrude roj hmab
Extruding roj hmab yog ib txoj kev ua uas siv cov extruder los extrude cov roj hmab sib tov mus rau hauv ib tug nruam sawb nrog ib tug tshwj xeeb cross-sectional duab. Cov txheej txheem no suav nrog cov kauj ruam hauv qab no:
Mixing: Sib tov roj hmab raw cov ntaub ntawv nrog additives los tsim ib tug roj hmab sib tov.
Pub: Pub cov roj hmab sib tov rau hauv qhov chaw pub noj ntawm lub extruder.
Cov cua sov: cua sov cov roj hmab sib tov los ntawm lub tshuab cua sov kom nws cov yas.
Extrusion: Extrude cov rhuab roj hmab sib tov los ntawm cov neeg kho tshuab lub taub hau los tsim ib tug nruam roj hmab nrog rau qhov xav tau cross-sectional duab.
Moulded Roj Hmab
Moulded roj hmab yog ib txoj kev ua uas yuav tsum tau muab cov roj hmab sib tov rau hauv pwm thiab shaping nws los ntawm lub siab thiab kub. Cov kauj ruam tseem ceeb suav nrog:
Npaj pwm: Tsim thiab npaj pwm nrog cov duab uas xav tau.
Mixing: Sib tov roj hmab raw cov ntaub ntawv nrog additives los tsim ib tug roj hmab sib tov.
Filling pwm: Sau cov roj hmab sib tov rau hauv pwm.
Cua sov thiab siab: Siv cov cua sov thiab siab kom ntws cov roj hmab sib tov thiab sau cov pwm, ua tiav cov txheej txheem molding.
Txias: Txias cov roj hmab hauv cov pwm kom khov rau hauv cov duab uas xav tau.
2. Kev sib piv ntawm cov yam ntxwv
Cov yam ntxwv ntawm extruded roj hmab
Nruam ntau lawm: Extruded roj hmab yog haum rau cov xwm txheej uas yuav tsum tau loj-scale nruam ntau lawm thiab muaj peev xwm ua tau npaum li cas lawm.
Complex cross-section: tuaj yeem tsim cov duab sib luag, tsim rau ntau yam khoom siv roj hmab.
Muaj peev xwm ntau lawm: Lub extruder muaj peev xwm ntau lawm thiab tsim nyog rau kev tsim khoom loj.
Cov yam ntxwv ntawm molded roj hmab
Cov duab raug: Moulded roj hmab tuaj yeem ua tiav cov duab meej dua, haum rau cov teb uas xav tau siab rau cov khoom zoo.
Kev tsim khoom me me: haum rau me me batch, customized ntau lawm, thiab tuaj yeem hloov kho raws li cov neeg siv khoom xav tau.
Surface zoo: Cov khoom tiav ntawm cov roj hmab molded feem ntau muaj qhov zoo ntawm qhov zoo thiab tsis tas yuav tsum tau kho deg ntxiv.
3. Daim ntawv thov teb
Daim ntawv thov teb ntawm extruded roj hmab
Sealing khoom: xws li roj hmab sealing strips, sealing rings, thiab lwm yam.
Cov yeeb nkab thiab fittings: Extruded roj hmab tuaj yeem siv los tsim cov khoom xws li cov kav dej thiab cov khoom siv.
Roj Hmab Sawb: Ib txoj hlua roj hmab siv rau hauv thaj chaw xws li kev tiv thaiv dej tsis zoo thiab tiv thaiv plua plav.
Daim ntawv thov teb ntawm molded roj hmab
Cov khoom siv hluav taws xob: Moulded roj hmab yog dav siv rau plua plav sealing ntawm cov khoom siv hluav taws xob.
Automotive Cheebtsam: xws li roj hmab pads, sealing rings, thiab lwm yam.
Cov khoom lag luam: Moulded roj hmab yog tsim rau ntau yam khoom lag luam uas xav tau cov duab meej thiab cov khoom zoo.