1. PVC (Polyvinyl Chloride)
PVC yog cov ntaub ntawv raw ofter siv nyob rau hauv kev npaj ntawm cov khoom kho mob yas, thiab nws cov nyiaj noj rau ntau tshaj 25% ntawm cov yas kho mob, Cov ntaub ntawv muaj cov nqi qis, cov ntaub ntawv thov dav thiab ntau yam yooj yim, thiab muaj cov tshuaj lom neeg zoo, cov khoom siv thiab hluav taws xob muaj zog, tab sis nws lub teeb tsis kam thiab thermal stability tsis zoo.
2. PE (Polyethylene)
Xws li LDPE, HDPE, UHMWPE, thiab lwm yam.
LDPE yog cov polyethylene uas tsis tshua muaj siab, Nws yog siv rau kev sib xyaw nrog lwm cov yas los tsim cov hnab ntim khoom kho mob thiab cov leeg txhaj tshuaj, thiab lwm yam.
HDPE yog qhov siab-polyethylene, Nws muaj cov khoom siv zoo, xws li lub ntsws ua kom zoo nkauj, lub ntsej muag dag, lub raum cuav, cov hlab tso zis, cov pob txha mos, cov khoom kho pob txha thiab cov khoom siv kho mob pov tseg, thiab lwm yam, thiab tuaj yeem siv los ua cov tshuaj txhawm rau txhim kho ntws cov yam ntxwv ntawm cov khoom.
UHMWPE yog ultra-high molecular phaus polyethylene.Nws muaj cov tshuaj lom neeg tsis tshua muaj siab, puas ua hauj, kev txhim kho corrosion thiab kev lom neeg tsis tuaj yeem.Nws yog cov khoom zoo rau kev tsim khoom lub ntsws thiab pob qij txha.
3. PP (Polypropylene)
Kev kho mob PP yuav tsum ua kom tau raws li qhov yuav tsum tau muaj siab huv, tsis muaj tshuaj lom, tsis muaj kuab lom, zoo tshuaj lom neeg ruaj khov, tsis muaj paug, tsis muaj mob, tsis haum tshuaj, tsis haum tshuaj zoo, tsis muaj mob carcinogenicity, tsis muaj hemolysis thiab coagulation, thiab lwm yam thiab tuaj yeem tiv thaiv kev kho mob ntawm cov tshuaj tua kab mob. ntawm ethylene oxide.
4. PTFE (TEFLON)
Polytetrafluoroethylene feem ntau yog siv hauv fluoroplastics, uas muaj siab crystallinity, tsis tshua muaj kev sib txhuam coefficient, kub zoo tsis kam, thiab muaj tshuaj lom neeg ruaj khov.Qhov khoom siv no tiv taus cov acids, alkalis, thiab ntau yam organic solvents.Almost insoluble hauv txhua cov kuab tshuaj.
5. TPU (Thermoplastic polyurethane)
Thermoplastic polyurethane muaj zoo pob tshab, lub zog siab thiab cov khoom tsim kua muag, tshuaj lom neeg kuj thiab cov ua hauj tsis kam; cov ntxig kuj muaj qhov ua tsis kam, thiab dej siab ua hauj ruaj khov.
6. PC (Polycarbonate)
Cov yam ntxwv ntawm polycarbonate yog cov tawv, lub zog, nruj thiab cov cua kub tiv thaiv kom tsis muaj menyuam.Qhov yam ntxwv no ua rau polycarbonate qhov kev xaiv zoo rau cov ntshav lim lim ntshav, kev siv tes ua haujlwm phais, thiab cov pa tso tsheb hlau luam.
7. TSIAJ (Polyphthalic acid)
Cov tshuaj lom neeg zoo thiab lub cev muaj zog ntawm PET tseem pw hauv nws txoj kev yoog tau zoo rau kev kho mob.Qhov muaj ntau yam ntawm PET hloov kho kom tau raws li qhov sib txawv ntawm cov khw kho mob plastics.
Cov yam ntxwv ntawm cov khoom siv kho mob yas:
Nws yog pom los ntawm kev tshawb fawb tias cov khoom lag luam yas muaj cov yam ntxwv nram qab no:
1. Lawv feem ntau yog tsim los ntawm kev rho tawm thiab txhaj tshuaj molding rau hauv cov khoom seem thiab tom qab ntawd ua theem nrab thiab sib dhos.
2. Muaj cov tshuaj lom txheeb ze rau kev ua tau zoo, piv txwv li: anticoagulation, super plam, tshuaj tua kab mob, thiab lwm yam.
3. Nws muaj cov haujlwm ua haujlwm sib txawv, xws li: hauv nruab nrab ntawm lub cev (venous cannula-lub taub hau yog muag muag, tiv thaiv sab hauv phab ntsa ntawm cov hlab ntsha.Qhov nqaij ntuag ntshav-lub taub hau yog qhov nyuaj thiab nws yooj yim nkag mus thaum phais.