Yuav ua li cas siv cov kev txhaj tshuaj qib siab los txo cov pov tseg hauv tsheb ntau lawm?

Txhim kho tus tsim ntawm cov pwm haus cov tshuab
Cov kev xaiv tsim nyog ntawm GATE hom thiab qhov chaw nyob
Tus Sprue yog cov channel los ntawm cov yas yaj nkag mus rau cov pwm kab noj hniav, thiab xaiv nws hom thiab txoj haujlwm muaj qhov cuam tshuam loj rau tiam neeg pov tseg. Ntau hom rooj vag yog haum rau cov ntaub ntawv yas sib txawv thiab cov khoom lag luam. Piv txwv li, tus kab mob yog qhov tsim nyog rau cov phab ntsa nyias thiab cov khoom yas me me. Nws tuaj yeem sau cov pwm kab noj hniav nrog cov khoom siv yas, txo cov khoom lag luam weld yog me me, ua kom yooj yim rau kev ua tiav thiab txo cov khib nyiab. Rau cov loj thiab complex zoo li cov khoom siv tsheb kho tsheb, xws li cov tsheb khiav tsheb, tus khiav kub khiav gating tuaj yeem siv. Tus khiav kub khiav kub tuaj yeem tswj qhov kub ntawm cov yas yaj hauv lub ntsej muag, zam lub ntsej muag ntawm lub rooj vag thiab txo lub cim ntawm lub rooj vag khib. Lub caij no, txiav txim siab lub rooj vag vim tsim nyog tuaj yeem ua kom muaj cov roj hmab txiv kab ntxwv, tsis txhob khib nyiab los ntawm kev siv khib nyiab los ntawm kev tsis txaus lossis ntau lub zos sau. Los ntawm kev siv simulation tsom software software, ntws ntawm yas yaj nyob rau hauv cov pwm kab noj hniav tau kwv yees, txoj haujlwm ua kom zoo.
Txhim kho cov txheej txheem channel
Tus khiav yog cov channel uas txuas rau Sprue thiab cov qauv siv hluav taws xob cuam tshuam nrog kev ua haujlwm zoo ntawm cov khib nyiab yas thiab ntau tiam neeg pov tseg. Kev tsim qauv tsoos channel feem ntau muaj teeb meem xws li ntau dhau ntawm cov khoom siv yas thiab kub thiab txias thaum lub sijhawm kub thiab txias thaum sov. Kev Txhaj Tshuaj Pwm Siab Txais yuav cov teeb meem Flun Channel Lej, tso cai rau cov kab noj hniav ib txhij thiab tsis sib xws, txo cov khoom pov tseg, txo cov khoom pov tseg vim tsis muaj kev sib xyaw ua ke. Tsis tas li ntawd, Channel ntu ua kom tsim nyog tuaj yeem xaiv los xaiv cov yam ntxwv tsim nyog ntawm cov yas thiab cov khoom lag luam xav tau kev ua tau zoo ntawm cov roj hmab yas thiab txo cov khib nyiab. Piv txwv li, siv cov channel ntws ncig tuaj yeem txo siab poob rau hauv cov channel thiab txhim kho kev ua kom yooj yim ntawm yas yaj.
Txhim kho kev tsim ntawm cov pwm tso tawm
Ua kom muaj kev ua kom txaus
Thaum lub sij hawm txhaj tshuaj molding cov txheej txheem, yog huab cua hauv cov pwm kab noj hniav tsis tuaj yeem sau rau hauv cov khoom yas, ua rau cov khoom lag luam yas, thiab lwm yam. Cov tshuaj tsis zoo no ua pov tseg. Cov qib siab txhaj tshuaj yog tsim nrog txoj kev tso pa tawm kom ntseeg tau tias huab cua hauv cov pwm kab noj hniav tuaj yeem raug tshem tawm tag nrho thaum lub tshuab molding cov txheej txheem. Cov txheej txheem kev tso tawm no suav nrog kev tso pa tawm, thiab lwm yam yog tsim los raws li cov yam ntxwv ntawm cov yas khoom thiab cov khoom xav tau. Kev tso rawv rau thaj chaw uas nws nyuaj rau teeb cov pa tawm, xws li sib sib zog nqus tej kab noj hniav. Los ntawm kev tsim cov tso tawm kev tsim nyog, cov khib nyiab tsim vim yog cov npuas tsis xws luag tuaj yeem txo.
Zam lwm cov teeb meem los ntawm kev tso tawm tsis zoo
Kev tso tsis zoo kuj tseem yuav ua rau muaj kev sib txig xws li txau thiab hlawv cov txiv hmab yas yaj thaum lub sijhawm ua tiav, ntxiv rau tiam neeg pov tseg. Txau yuav ua rau cov yas yaj kom ncaj qha cuam tshuam cov kab noj hniav phab ntsa, ua rau muaj kev txo qis hauv cov khoom lag luam zoo; Kev hlawv hlawv yog tshwm sim los ntawm oxidation tshuaj ntawm yas yaj nyob rau hauv kev sib cuag nrog huab cua ntawm cov khoom dub kub, ua rau cov pob dub nyob rau ntawm cov khoom. Kev Txhaj Tshuaj Yooj Yim zam cov teeb meem no los ntawm kev txhim kho cov txheej txheem thiab cov qauv ntawm cov tso pa tawm. Piv txwv li, siv cov kev tso tawm class ua rau huab cua kom yooj yim thaum txo cov tole ntawm yas yaj.
Tsim Tsim Kev Ua Haujlwm Pwm Txias Txheej Txheem Thov
Uniform Txias Kom Xob Txo Cov Khoom Muag Discormation
Cov khoom lag luam tawm yog ib qho teeb meem zoo hauv kev txhaj tshuaj molding cov khoom lag luam, thiab deformed cov khoom lag luam feem ntau tsis ua raws li kev sib dhos thiab ua pov tseg. Kev Txhaj Tshuaj Pwm Adjected yuav ua ib qho kev hloov kho lub kaw lus los xyuas kom meej tias cov yas yaj yog cov khoom siv yas ua kom txias hauv cov lus ci. Los ntawm kev tsim kho cov dej txias dej ntws hauv cov pwm uas txias ntawm cov khoom sib txawv ntawm cov khoom lag luam sib txawv ntawm cov khoom lag luam thiab li txo qhov kev pheej hmoo ntawm cov khoom lag luam deformation. Piv txwv li, los ntawm kev siv cov dej ua ke txias channel thiab tsim cov khoom siv cua txias tuaj yeem ze rau saum npoo ntawm cov khoom, txhim kho kev ua haujlwm txias thiab txo cov khoom lag luam tawm.
Tswj lub sijhawm txias thiab kub
Kev tswjfwm ntawm lub sijhawm txias thiab qhov kub kuj tseem muaj kev cuam tshuam tseem ceeb ntawm kev ua tau zoo thiab khib nyiab ntawm cov khoom. Yog tias lub sijhawm txias yog luv heev, cov khoom yuav tsis raug tshuaj tag nrho, thiab nws yog ib qho tsis yog deformation lossis kev puas tsuaj thaum lub sij hawm nyuaj; Yog hais tias lub sijhawm txias yog ntev dhau lawm, nws yuav txo cov peev txheej ntau lawm. Kev tswj hwm cov pwm hluav taws xob tau nruab nrog tswj qhov ntsuas kub uas tuaj yeem tswj cov dej txias, txiav txim siab cov yam ntxwv ntawm cov khoom siv yas thiab cov khoom lag luam. Los ntawm kev ua kom zoo dua txias, khib nyiab tsim vim yog qhov txias tsis huv tuaj yeem txo thaum txhim kho kev ua haujlwm tau zoo.
Txais yuav tau kho tau thiab moulular pwm tsim
Haum rau Ntau Ntau Yam Ntau Lawm
Hauv cov tsheb tsim, nws yog feem ntau tsim nyog los tsim cov qauv yas ntawm cov qauv sib txawv thiab cov kev qhia tshwj xeeb. Cov tshuaj tua ib txwm muaj feem ntau nyuaj los hloov kho cov kev xav tau sib txawv ntau yam, ua rau cov pwm hloov pauv thiab nce pov tseg ntau tiam. Kev tau txais kev txhaj tshuaj pwm tsim kho kom tau thiab kho qauv, uas tuaj yeem hloov kho tau sai rau kev tsim cov khoom sib txawv. Piv txwv li, cov tub ntxhais thiab kab noj hniav ntawm cov pwm tuaj yeem siv cov khoom siv hloov tau, thiab los hloov cov qauv sib txawv, cov qauv sib txawv tuaj yeem tsim tawm. Cov qauv tsim no txo qhov rov ua dua cov pwm ntawm cov pwm, cov nqi ntau lawm, thiab kuj txo cov khoom pov tseg vim tias hloov pwm.
Yooj yim kho thiab tswj pwm
Pwm yog inevitably nquag hnav thiab kev puas tsuaj thaum siv, thiab xav tau kho lub sijhawm thiab kho. Adjustable thiab mouldular mould tsim ua kom muaj kev tu pwm thiab rub tawm yooj yim dua. Thaum ib feem ntawm pwm ua malfunctions, tsuas yog qhov sib raug zoo yuav tsum tau hloov, tsis tas yuav disassemble thiab kho kom tag nrho cov pwm, txo lub sijhawm tu thiab nqi. Lub caij no, cov qauv tsim qauv kuj tau yooj yim rau kev txhim kho thiab txhim kho pwm, txhim kho lawv cov kev ua tau zoo thiab kev txo cov nyiaj pov tseg.
Los ntawm kev siv tshuaj ntsuam txuj ci siab los ua kom zoo dua ntau yam xws li siv cov kab ke, tso tawm, pov tseg hauv kev tsim kho tsheb, cov khib nyiab hauv kev txo qis hauv tsheb tuaj yeem raug txo kom zoo. Qhov no tsis tsuas pab txo cov nqi ntau lawm thiab txhim kho kev txhim kho kev lag luam, uas yog qhov tseem ceeb rau kev txhim kho ntsuab ntawm kev lag luam kev lag luam. Nrog kev nce qib nruam ntawm thev naus laus zis, kev txhaj tshuaj pwm thev naus laus zis yuav txuas ntxiv ua kom thev naus laus zis ntxiv, muab cov kev daws teeb meem ntau dua.