Yuav Ua Li Cas Txhaj Pwm Tsim Tiv Thaiv Npuas thiab Voids hauv cov khoom yas?

Peb Hom "Bubbles" thiab Vim Li Cas Lawv txawv

Thaum ib tug neeg hais tias lawv feem muaj npuas, lawv feem ntau txhais tau tias yog ib qho ntawm peb yam, thiab sib xyaw ua ke ua rau caum qhov kho tsis raug.

Cua ntxiab: hnab tshos ntawm cua ntxiab uas cov yas molten tsis tuaj yeem thawb tawm ntawm pwm

Voids: lub tshuab nqus tsev npuas uas tsim hauv cov ntu tuab raws li cov yas txias thiab shrinksMotor Iav Txhaj PwmMotor Iav Txhaj Pwm

Moisture npuas (splay): silvery streaks los yog npuas tshwm sim los ntawm dej hauv cov yas ua ntej molding

Txhua tus zoo li txawv me ntsis thiab los ntawm qhov sib txawv kiag li. Cua ntxiab tshwm sim vim cov pwm tsis tuaj yeem ua pa. Voids tshwm sim vim cov phab ntsa tuab thiab shrinkage. Cov npuas npuas tshwm sim vim cov khoom tsis qhuav. Txheeb xyuas qhov twg koj muaj ua ntej, tom qab ntawd kho qhov laj thawj tshwj xeeb.

Cua ntxiab: Thaum Pwm tsis tuaj yeem ua pa

Thaum molten yas rushes rau hauv pwm kab noj hniav, nws thawb cua ua ntej ntawm nws. Huab cua ntawd yuav tsum mus rau qhov chaw. Yog tias cov pwm tsis muaj qhov cua kom dim, cov yas ntxiab nws, thiab koj tau txais npuas lossis kub hnyiab qhov chaw uas huab cua tau compressed thiab overheated.

Qhov no yog ib qho ntawm feem ntau ua npuas ncauj, thiab nws tsuas yog ib qho teeb meem tsim pwm. Cov peev txheej txheej txheem los ntawm Lub Koom Haum ntawm Plastics Engineers tsis tu ncua taw qhia txog qhov ua pa tsis txaus ua qhov ua rau muaj kev cuam tshuam rau cov khoom siv hluav taws xob tsis zoo -. Cov huab cua feem ntau tau daig ntawm qhov chaw kawg los sau, feem ntau yog lub ces kaum, tav tav, lossis qhov kawg ntawm txoj kev ntws.

Hauv cov teeb meem ntawm kev txhaj tshuaj molding gas, qhov qhia -tale kos npe yog ib qho kev kub hnyiab me me lossis qhov khoob uas ib txwm tshwm sim hauv tib qhov chaw, tua tom qab txhaj tshuaj. Qhov kev rov ua dua ntawd qhia koj tias nws yog qhov teeb meem venting, tsis yog txheej txheem random glitch.

Venting Design: Qhov Kho Tiag Tiag rau Huab Cua Traps

Kev daws rau cov cua ntxiab yog qhov ua kom zoo, uas txhais tau hais tias muab cov cua ntxiab hauv txoj hauv kev kom dim uas me me dhau rau cov yas ua raws. Zoo venting tsim kev txhaj tshuaj molding muaj xws li:

Vents muab tso rau ntawm qhov chaw kawg los sau, qhov twg huab cua sib sau

Qhov qhov tob tob tob txaus kom tso cua tawm tab sis tsis yog yas (feem ntau yog ob peb puas ntawm ib millimeters)

Vents ntawm ejector pins, uas ua ob npaug li huab cua khiav txoj kev

Qhov chaw nyob hauv qab ntawm cov tav sib sib zog nqus thiab cov thawj coj

Txoj kev ua pa kom zoo ua rau huab cua txhua txoj hauv kev tawm ntawm pwm

Rau ibTsav Iav Txhaj Pwm, cov hniav iav thiab qhov chaw nruab nrab ntawm lub hub thiab lub npoo yog cov chaw uas yuav tsum tau ceev faj qhov cua. Peb daim ntawv qhia cov qauv sau thaum tsim los kwv yees qhov twg huab cua yuav xaus, tom qab ntawd muab cov vents rau ntawd ua ntej cov hlau txiav. Ntxiv vents tom qab qhov tseeb yog ua tau tab sis yeej tsis huv li tsim lawv los ntawm qhov pib.

Yog vim li cas Thick Sections Trap Nqus Npuas Npuas

Voids txawv. Lawv tsis yog daig cua. Lawv yog lub tshuab nqus tsev npuas uas tsim thaum ib ntu tuab ntawm cov yas txias.

Nov yog qhov tshwm sim. Sab nraud ntawm ib ntu tuab txias thiab solidifies ua ntej, tsim daim tawv nqaij. Sab hauv tseem molten. Raws li nyob rau hauv txias, nws shrinks, tab sis cov tawv nqaij tawv tuav nws cov duab. Lub shrinking sab hauv rub tawm ntawm nws tus kheej thiab tsim ib tug hollow void nyob rau hauv qhov chaw. Lub thicker seem, qhov phem nws tau txais.

Lub cev muaj zog iav nrog lub hub tuab yog ib tus neeg sib tw classic. Lub hub yog qhov tuab tshaj plaws ntawm cov iav, yog li nws yog qhov chaw tsis muaj ntaub ntawv. ASTM D3417 thiab lwm yam thermal- txoj kev tshuaj ntsuam piav qhia txog yuav ua li cas crystalline plastics shrinks thaum lawv txias, thiab qhov shrinkage yog raws nraim li cas drives void tsim nyob rau hauv tuab seem.

Phab ntsa Thickness thiab Coring Solutions

Kev kho rau voids yog kom tsis txhob muaj cov khoom tuab tuab hauv thawj qhov chaw. Cov kev cai tsim yog ncaj nraim:

Khaws phab ntsa tuab kom zoo ib yam li ua tau thoob plaws ib feem

Core tawm cov ntu tuab kom lawv ua hollow es tsis yog khoom

Qhov twg lub hub tuab yog yam tsis muaj kev zam, rov tsim nws nrog lub chaw cored thiab tav rau lub zog

Khaws cov tav ntawm kwv yees li 60% ntawm cov phab ntsa loj kom tsis txhob tsim cov pob tuab tshiab

Ntawm no yog ib tug scenario peb pom ntau zaus. Ib tus neeg siv khoom nqa peb lub iav nrog cov khoom tuab tuab, vim qhov ntawd yog li nws tau kos hauv CAD. Moulded li -yog, lub hub ua ib qho khoob txhua lub sijhawm. Kev kho yog txhawm rau txhawm rau hauv nruab nrab ntawm lub hub thiab ntxiv kev txhawb nqa tav, uas ua kom lub zog thaum ua rau phab ntsa nyias txaus kom txias yam tsis muaj qhov khoob. Qhov no yog ib qho kev hloov pauv, thiab nws yog qhov pheej yig dua los ua rau ntawm qhov screen dua li khiav hauv pem teb molding nrog cov txheej txheem tweaks uas yeej tsis ua haujlwm tag nrho.

Kev tiv thaiv tsis zoo molding feem ntau yog hais txog kev tsim phab ntsa. Cov txheej txheem tuaj yeem pab ntawm cov npoo, tab sis koj tsis tuaj yeem ntseeg tau koj txoj hauv kev tawm ntawm ib feem uas muaj cov khoom tuab hauv nws.

Moisture Bubbles: Qhov Teeb Meem Qhuav

Qhov thib peb hom npuas tsis muaj dab tsi ua nrog pwm txhua. Qee cov yas nqus dej noo los ntawm huab cua. Yog tias koj pwm lawv yam tsis tau ziab ua ntej, cov dej yuav tig mus rau hauv lub thoob thiab pom zoo li cov nyiaj streaks lossis npuas rau ntawm qhov chaw. Qhov teeb meem no hu ua splay.

Kev kho yog yooj yim tab sis feem ntau hla: qhuav cov khoom kom zoo ua ntej molding, ua raws li cov khoom siv cob qhia qhov kub thiab lub sijhawm. Cov ntaub ntawv zoo li nylon, PC, thiab ABS tshwj xeeb tshaj yog rau qhov no. Yog tias koj cov npuas zoo li silvery thiab tshwm sim tawg thoob plaws hauv qhov chaw es tsis yog nyob rau hauv ib qho chaw ruaj khov, xav tias ya raws ua ntej koj cem cov pwm.

Yuav ua li cas peb tsim iav pwm yam tsis muaj Voids

Peb txoj hauv kev yog los tiv thaiv tag nrho peb hom npuas ua ntej pwm tsim. Thaum lub sij hawm tsim-rau- kev tshuaj xyuas kev tsim khoom, peb khiav ib qho kev tshuaj ntsuam xyuas los kwv yees cov cua ntxiab thiab tso qhov cua qhov chaw uas huab cua yuav sau. Peb tshuaj xyuas cov phab ntsa thickness thiab core tawm txhua ntu tuab uas yuav ua rau voids. Thiab peb qhia meej qhov tseeb ziab rau cov khoom xaiv.

Rau qhov tseeb ib yam li lub cev muaj zog, qhov nce ntawm - ua haujlwm pem hauv ntej yog dab tsi muab rau koj qhov chaw uas muaj suab nrov thoob plaws, tsis yog ntawm qhov chaw xwb. Ib qho khoob uas koj tsis tuaj yeem pom yog qhov txaus ntshai tshaj plaws, vim tias nws dhau qhov kev kuaj pom thiab ua tsis tiav hauv daim teb.

F AQ

Q: Dab tsi ua rau npuas hauv txhaj tshuaj molded qhov chaw?

A: Muaj peb qhov laj thawj tseem ceeb. Cua ntxiab los ntawm pwm uas tsis tuaj yeem tso cua ua ntej ntawm cov yas ntws. Voids yog lub tshuab nqus tsev npuas uas tsim hauv cov ntu tuab thaum lawv txias thiab ntsws. Cov npuas npuas los ntawm cov yas molding uas tsis tau qhuav ua ntej. Txhua tus muaj qhov sib txawv, yog li kev txheeb xyuas qhov koj muaj yog thawj kauj ruam.

Q: Kuv Yuav Ua Li Cas Tiv Thaiv Huab Cua Hauv Kev Txhaj Tshuaj Molding?

A: Cov cuab yeej cua yog tiv thaiv los ntawm kev ua kom zoo hauv cov pwm. Vents mus qhov twg cov huab cua sib sau, feem ntau yog cov chaw kawg los sau, thiab lawv loj kom tso cua tawm tab sis tsis yog yas. Zoo venting tsim kev txhaj tshuaj pwm ua hauj lwm maps cov qauv sau ua ntej, ces muab cov vents ntawm lub ntxiab ntsiab lus ua ntej pwm txiav.

Q: Vim li cas Kuv Cov Khoom Yas Uas Muaj Qhov Ncauj Hauv Ib Cheeb Tsam?

A: Vim tias cov ntu tuab txias tsis sib xws. Sab nraud solidifies ua ntej, thiab raws li qhov tseem -molten center cools thiab shrinks, nws rub tawm thiab tawm ib tug hollow void. Txoj kev kho yog kom cov tub ntxhais tawm ntawm cov ntu tuab kom cov phab ntsa ua ib yam. Qhov no feem ntau tshwm sim hauv qhov chaw xws li iav hubs, uas yog vim li cas lub qhov dej -tsim lub cev muaj zog Gear Txhaj Pwm cores lub hub es tsis tso nws cov khoom.

Q: Cov txheej txheem tuaj yeem txhim kho npuas, lossis Nws Puas Yog Pwm?

A: Nws nyob ntawm qhov ua rau. Cov npuas npuas yog tsau los ntawm ziab cov khoom. Cua ntxiab thiab voids feem ntau yog pwm thiab tsim teeb meem, txawm hais tias tuav lub siab thiab lub sij hawm txias tuaj yeem pab ntawm cov npoo. Yog tias koj pom koj tus kheej khiav cov txheej txheem huab cua tsuas yog txhawm rau txo cov npuas, qhov teeb meem tiag tiag feem ntau yog nyob rau hauv pwm lossis ib feem tsim.

Q: Qhov twg Kuv Yuav Nrhiav Tau Lub Cav Txhaj Tshuaj Txhaj Tshuaj Pwm Chaw Tsim Tshuaj Leej Twg Tiv Thaiv Cov Voids?

A: Saib rau tus neeg muag khoom uas sau cov kev tshuaj ntsuam xyuas thiab tshuaj xyuas cov phab ntsa thickness thaum lub sij hawm tsim, ua ntej txiav steel. Lub Hoobkas uas tsim cov qhov cua thiab cov cores tuab ntu pem hauv ntej yuav muab rau koj qhov chaw suab. Ib qho uas tsuas yog hais txog npuas tom qab thawj qhov kev sim ua tsis tiav yog twb tom qab.

Pib koj qhov phiaj xwm Gear Pwm yam tsis muaj teeb meem npuas

Yog tias koj tab tom nrhiav lub Tsav Tsav Tsheb Txhaj Tshuaj Pwm lossis ib feem nrog cov ntu tuab thiab kev ua haujlwm lub zog, lub sijhawm los tiv thaiv npuas thiab voids yog thaum tsim, tsis yog tom qab thawj zaug sim. Xa koj qhov chaw rau peb thiab peb yuav khiav tus qauv tsim dawb-rau- kev tshuaj xyuas kev tsim khoom.

Hu rau tam sim no

Xa kev nug

Tsev

Xov tooj

Tug

Kev nug